Material Notes:
Industry Application: High StrengthProduct Application: MilitaryDistinct Features: High Impact Low Profile; Paintable/In Mold Coatable; Low Shrink; Low Moisture Absorption; Bondable; Formulated for High Stress and VibrationInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Tensile Strength, Ultimate 103 MPa
15000 psi
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
Tangent; ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256