Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler
(discontinued **) Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa.. |
|||
Density | 1.61 - 1.65 g/cc | 0.0582 - 0.0596 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 337 Rigid PVC, Extrusion Cheap profiles |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific) LNP* LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT (Asia Pacific) LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific) LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Polyplastics Duranex® CRN7015 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-240 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | |
A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | |
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Density | 1.61 - 1.65 g/cc | 0.0582 - 0.0596 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 9030 Flexible PVC, Lead Free Various profiles |