Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.45 g/cc | 0.0524 lb/in³ | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
Momentive Performance Materials TSE326 Red Adhesive Sealant, Non-Corrosive Flowable High Temperature One-part heat cure. Typical uses: Assembly and gasketing.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
LATI Latilub 80-10T K/15 PPS, 15% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF/M38 HS 38% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 38% Filler by Weight and Mineral Filler, 38% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabili.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES (Asia Pacific) LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C140 BK086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding. It has very low warpage.Information provided by Du.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 3380 & CORE 1 Polyester Film Melinex® 3380 and Melinex® CORE1 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
DuPont Teijin Films Melinex® CORE 1 & 3380 Polyester Film Melinex® CORE1 and Melinex® 3380 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
E-Polymers TEKAMID® TA250GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Density | 1.45 - 1.60 g/cc | 0.0524 - 0.0578 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
A. Schulman ComAlloy Comtuf® 639 Nylon 6/6, Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Mineral reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183/A |
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
BASF Paliogen® Red L 3910 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
A. Schulman ComAlloy Hiloy® 638 Nylon 6/6, Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.45 - 1.50 g/cc | 0.0524 - 0.0542 lb/in³ | |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |