Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183-1 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Density | 1.43 g/cc | 0.0515 lb/in³ | |
Lord Adhesives 306 High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Electrablend® POM CF15 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerAppearance: Natural ColorInformation provided by TP Composites, Inc... |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA4/6 GF33 HS NAT 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PET GF15 X BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF007 PA 6 LNP* THERMOCOMP* PF007 is a compound based on Nylon 6 resin containing 35% Glass Fiber. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear LNP* THERMOCOMP* OC006 is a compound based on PPS-Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 011 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 83 Flexible PVC, Sheathing General purposes |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NT40 GR30 NL HS PPA, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
3M Scotch-Weld™ AC09 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC09 is a fluorinated solvent based activator that is non-flammable.Information provided by 3M |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin 15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D1505 |
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade Data provided by PolyOne. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Polyplastics Duracon® EB-10 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |