Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.38 g/cc | 0.0499 lb/in³ | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-HG6U (Cond.) 33% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo.. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding Fittings high fluidity |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | |
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | |
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF33 LE 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Extraction ResistantProcessing Method: Injection MoldingInformation provided b.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF33 LE BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesAppearance: BlackTPCI#7762101Information provided by TP Compos.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific) LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | dry; ISO 1183 |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 54G35EF BKB336 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced laser markable PPA High Performance Polyamide Developed for Electrical and Electronics Applications. Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabiliz.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i.. |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 HI2 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding Electric antishock fittings |
|||
Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu.. |
|||
Density | 1.38 - 1.42 g/cc | 0.0499 - 0.0513 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 93 Flexible PVC, Sheathing Lead Free Sheathing automotive cables |