Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 - 1.45 g/cc | 0.0408 - 0.0524 lb/in³ | Average value: 1.34 g/cc Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hysun™ A598 ASA Polycarbonate alloy
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Density | 1.13 - 1.14 g/cc | 0.0408 - 0.0412 lb/in³ | Average value: 1.14 g/cc Grade Count:10 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | Average value: 1.14 g/cc Grade Count:8 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® 996 Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at t.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | DIN 53479 |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 L UV (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | |
Solvay SOPROPHOR® 4 D 384 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: POLYARYLPHENYL ETHER SULPHATE, AMMONIUM SALTSolubility: Soluble in water and most polar and aromatic solvents.Available .. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | JIS-Z-8807 |
Denka LCS Z1060 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced Information provided by Entec |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**) Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Density | 1.13 g/cc @Thickness 2.00 mm |
0.0408 lb/in³ @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D792 |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |