Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.09 g/cc | 0.0394 lb/in³ | NCMT Method |
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.09 - 1.46 g/cc | 0.0394 - 0.0527 lb/in³ | Average value: 1.23 g/cc Grade Count:23 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP AL001 ABS LNP LUBRICOMP* AL-4010 HP is a compound based on Acrylonitrile Butadiene Styrene resin containing 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont |
|||
Density | 1.09 g/cc | 0.0393 lb/in³ | |
Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Momentive Performance Materials RTV142 White Adhesive Sealant, Non-Corrosive Paste One-part cure. Typical uses: Low volatile adhesive; use as electronic gasketing adhesive for critical aerospace applications.Data provided by the manufacturer, GE Silicones.GE Silicones became a pa.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 230 PA6, Conditioned Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AX90213 ABS LNP* THERMOCOMP* AX90213 is a compound based on ABS resin containing Glass Fiber. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Solvay GEROPON® CYA/75 Surfactant Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN HYDRO ALCOHOLIC SOLUTIONCAS: 577 – 11 – 7 / 64 – 17 – 5Solubility: Dispersible in water and polar solvents. Soluble in most aroma.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/B |
Styron PULSEâ„¢ GX50 PC/ABS Engineering Resin Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin pr.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Solvay SOPROPHOR® S/25 Surfactant Description: Soprophor® S/25 is Tristyrylphenol ethoxylate, HLB = 14.5. It is nonionic multipurpose high performance emulsifier, soluble in water and most polar and aromatic solvents. Recommended.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Master Bond MB297 Cyanoacrylate Adhesive System General purpose, fills gap to 0.008Information provided by Master Bond Inc. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
Chase Plastics CP Pryme® NN100TL (Dry) Nylon 66, Lubricated, Impact Modified Features: LubricatedImpact modifiedGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | DIN 53479 |
Polyram PlusTek RA843 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Loctite® 496 General Purpose Methyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
Entec Hypro™ PPC-GF25 Natural Impact Polypropylene, 25% Glass Reinforced Information provided by Entec |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 NL IL PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
3M Scotch-Weld™ MG6500-74 UV/VIS Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
Addiplast Addinyl C2 R Nylon 66/6 High impact resistanceInformation provided by Addiplast. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | |
Solvay RHODISOLV® RPDE Solvent Rhodiasolv RPDE is an environment friendly, biodegradable, non toxic, non ecotoxic, low VOC solvent.Identification: DIMETHYL GLUTARATE, DIMETHYL SUCCINATE, DIMETHYL ADIPATECAS: 627 – 93 – 0 / 1119.. |
|||
Density | 1.09 - 1.56 g/cc | 0.0394 - 0.0564 lb/in³ | Average value: 1.22 g/cc Grade Count:149 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Density | 1.09 g/cc | 0.0394 lb/in³ | Latex |
DuPont Performance Polymers AquaStik® AQS-1120 Polychloroprene Latex
(discontinued **) Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features mechanical stabil.. |