Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Nylene® PA6/6 Impact Modified 4120 HS Nylon 6/6; MoS2 lube High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Polykemi AB POLYsan PN127 Styrene Acrylonitrile Information provided by Polykemi AB |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B52^ E Nylon 6, Modified Information provided by Polykemi AB |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Plastcom SLOVAMID 6 MI/2 PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D 792 |
Shakespeare Isocorâ„¢ TT65SI Nylon 6 Terpolymer Isocorâ„¢ TT65SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocorâ„¢ TT65SI is soluble in common al.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Styron EMERGEâ„¢ 5100 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided b.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Solvay ALBRITECT® CP 30 Vinyl phosphonic acid - acrylic acid copolymer, 20% Aqueous solution VINYL PHOSPHONIC ACID – ACRYLIC ACID COPOLYMER (20% SOLUTION IN WATER) CAS: 27936 – 88 – 5Solubility in Water: Miscible (in all proportions)Available in: Asia Pacific, Europe, Latin A.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Styrolution Absolan® 2300 SAN Absolac 2300 is a good flow gradeInformation provided by Styrolution |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Silon TA 2347 HD Orange Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2347 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | DIN 53479 |
Polyram PlusTek PA880 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.08 g/cc @Temperature 300 °C |
0.0390 lb/in³ @Temperature 572 °F |
Melt |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM Data |
Dow Tyril® 880 SAN TYRIL® 880 SAN copolymer offers excellent physical properties incorporating the highest levels of chemical resistance, heat resistance and overall strength of any TYRIL grade.Data provided by Dow C.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | Accelerator |
3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives 3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and .. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | Uncured |
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
BASF Basantol® 099 Yellow Liquid Chemical Structure: Quinophthalone dyeColour Index: Direct Yellow 5Application: Dye for wood stainsPhysical Form: LiquidInformation provided by BASF |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermotuf V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
Buckeye Polymers BP RPP 2520 CU Polypropylene, 25% Mineral Filled UV StabilizedCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition.. |