Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-0863 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D1505 |
SABIC CC862 High Density Polyethylene for Injection Molding Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal c.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Huntsman Rexell® H2105 Injection Molding LLDPE
(discontinued **) Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting and Profile ResinCharacteristics: High Melt Strength - Larger Parts, Wide Range of Processing Conditions, High Stiffness and Impact Resistance,.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-166 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1183 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | |
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis Borcell™ HE1123 High Density Polyethylene Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 72 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 73 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AA60-003 Blow Molding Resin Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AD60-005 Blow Molding Resin Product Description: AD60-005 is a medium molecular weight districution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AD60-007 Blow Molding Resin Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | |
Dow HDPE 05862N High Density Polyethylene Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D-792 |
Bapolene® 3257U Polyethylene, Injection Molding Bapolene 3257U is a high density polyethylene resin that offers improved cycle times, superior modulus and impact resistance. It complies with US FDA 21CFR177.1520 and has a UV protection package.A.. |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin
(discontinued **) 4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical |
|||
Density | 0.963 g/cc | 0.0348 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 71 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |