Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Finathene® 6002 HDPE, blow molding, pipe
(discontinued **) FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Finathene® 7208 HDPE extrusion resin
(discontinued **) Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Lacqtene® 2005 TN 59 HDPE pipe
(discontinued **) LACQTENE® 2005 TN 59 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2005 TN 59 is best processed between 190 and 230°C.Informa.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1C61 UV Cure Conformal Coating Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D792 |
LyondellBasell Alathon® L5906 High Density Polyethylene ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Density | 0.959 - 0.965 g/cc | 0.0346 - 0.0349 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GD 5160 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.959 - 1.01 g/cc | 0.0346 - 0.0364 lb/in³ | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.959 - 0.983 g/cc | 0.0346 - 0.0355 lb/in³ | |
Lord Adhesives Flocklok® Catalyst 1 Flocklok Catalyst 1 will accelerate the cure rate of Flocklok adhesives and will not diminish the work life, unless exposed to moisture. There is minimal impact on VOC levels, as low levels of the c.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Density | 0.959 g/cc @Temperature 20.0 °C |
0.0346 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PMA Propylene glycol methyl ether acetate Available in electronic grade.Information provided by Lyondell. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Compound; ISO 1183 |
Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings BorSafe™ HE3490-IM is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | compound; ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Xsene® BM 593 HDPE, blow molding FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been es.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792 |
Dow CONTINUUM™ DGDC-2480 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | |
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | AboCure 50-4 |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Density | 0.959 - 3.12 g/cc | 0.0346 - 0.113 lb/in³ | Average value: 1.94 g/cc Grade Count:17 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |