Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin
(discontinued **) Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D4883 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Finathene® SR 572 HDPE blow molding
(discontinued **) FINATHENE® SR 572 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® SR 572 has been developed for the manufacturing of blow molded bottles .. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin Features: Good ESCR, high stiffness, good impact strength.Applications: Small part blow molding, HIC containers, food, pharmaceuticals.Data provided by the manufacturer. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
Global R-1760 High Density Polyethylene, Injection Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 60505 High Density Polyethylene 60505 is a HDPE injection molding grade which combines high stiffness with good physical properties. This resin is well suited for crates and toys applications.Application: crates, injection molding.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) I1 HA 7260 High Density Polyethylene I1 (HA 7260) is a high density polyethylene with propylene as comonomer. It is very easy flowing, high density, hardness and stiffness, largely warpage free, for mass product articles in rapid shot .. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene R1760 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending .. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high dens.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance... |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | |
JPJ Technologies 3000j/JE HDPE Injection Information provided by JPJ Technologies |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding Applications:Large dustbins and pailsPallet boxesFish cratesTechnical moldingInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB 68 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792-ISO 1183, ASTM D1505 |
DuPont Elvax® 150 Ethylene Vinyl Acetate DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D-1505 |
Chevron Phillips Marlex® 9514H Polyethylene; HDPE High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: Require excellent stiffness to ESCR ratioRequire good m.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 02133EN2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02133EN12 is a copolymer of ethylene and vinyl acetateAvailability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoFree Flowing Agent:.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D4883 |
ExxonMobil HD 9856B Blow Molding Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem GM5240PR HDPE High Density Extrusion Polyethylene GM5240PR is a high-density polyethylene compound specially developed for the manufacturing of pipes, underground conduits, and steel pipe coating. This resin is produced with bimodal technology and .. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Braskem JV 060U HDPE Injection Molding Polyethylene Applications: Caps, crates for industrial, transportation or fishing uses, industrial pails, stands and pallets, refuse containers; bottle cases, safety helmets, cages for poultry transportation and.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene V1160 High Density Polyethylene CHARACTERISTICS: GOOD FLOWABILITYAPPLICATIONS: INJECTION MOLDING FOR LIGHT WEIGHT HOUSEHOLDS, TOYS, FOOD CONTAINERS, COSMETICS CLOSURES, DISPOSABLE ARTICLES, LARGE MOLDING AND COMPLICATED PARTS |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th.. |