Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.950 g/cc | <= 0.0343 lb/in³ | ISO 1183 |
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | STN EN ISO 1183-1 |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183-A |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Orbilan RubberLen® R55 HMW-PE, dark blue ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total Evatane® 28 - 03 HDPE, blown film
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Density | 0.950 - 1.14 g/cc | 0.0343 - 0.0414 lb/in³ | Average value: 1.03 g/cc Grade Count:43 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Density | 0.950 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | |
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene Production Method: Gaseous-phase method. Application: Compositions are intended for cover insulating lapping, protective covers and cables.Information Provided by Kazanorgsintez |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | Not Compounded |
KKPC KOSYN 1712L Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
Styron Buna® SB 1739 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Composition: Buna® SB 1739 – Schkopau is manufactured by cold polymerization using mixed rosin acid /fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE o.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
Solvay RHODAPHOSE® TG PHOS REAGENT Phosphorus Derivative Description: Phosphitylating reagent used typically in the manufacture of amidite monomers for synthetic RNA sequencing.Identification: 2-CYANOETHYL N,N,N’,N’-TETRAISOPROPYLPHOSPHORODIAMID.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Borealis Borstar® HE3477-LS Red-Brown Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Sewerage Borstar HE3477-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MS 57 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D 792 |
Total 50100.2 HDPE blow molding, sheet, thermoforming resin Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging, sheet extrusion, thermoforming, truck bed liners, dunnage containers.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® E265 Polymer Modifier DuPont™ Fusabond® E265 is an anhydride modified high density polyethylene. Used as a polymer modifier |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. ORE.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Arkema Group Orevac® 9305 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Hot melt adhesivesInformation provided by Arkema Group |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced |
|||
Density | >= 0.950 g/cc | >= 0.0343 lb/in³ | UNI EN ISO 1183-1 |
Breplast Bretene TS COR Plus High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Density | >= 0.950 g/cc | >= 0.0343 lb/in³ | UNI EN ISO 1183-1 |
Breplast Bretene TS COR White F60 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ EX49-006 Extrusion Grade Resin
(discontinued **) EX49-006 is an unstabilized high density polyethylene extrusion grade polyethylene copolymer. It is designed for blending and compounding with fillers, such as wood flour, to give uniform mixing an.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183-A |
Okulen® 500 PE-HMW, Natural OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |