Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Polymer Industries Densetec HMW Sheet Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is mor.. |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4850B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Reliance Industries Relene D16501 Polyethylene Relene D16501 is a UV stabilized High Density Polyethylene compound with broad molecular weight distributions, suitable for producing cable duct for optic fiber and other general purpose cables. Th.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® ETP H5057 High Density Polyethylene ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit.. |
|||
Density | 0.948 - 0.954 g/cc | 0.0342 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4950 HS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |
|||
Density | 0.948 - 0.954 g/cc | 0.0342 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D792 |
Sterigenics Raprex® R-100 Branched High Density Polyethylene Applications: ExtrusionRAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ISO 1183 |
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ISO 1183 |
Borealis Borstar® HE3474-LS Blue HDPE Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Drinking Water Borstar HE3474-LS is a bimodal, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die build-up duri.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | base resin; ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D792-ISO 1183, ASTM D1505 |
DuPont Elvax® 350 Ethylene Vinyl Acetate DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 15028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 40028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil HDPE AA48-002 High Density Polyethylene Resin Product Description: AA48-002 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a very good balance of stress crack resistance, stiffness and.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin Product Description: HD 6601 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance... |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D792 |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | |
Dow DOWLEX™ IP-42 High Density Polyethylene DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 613 HPE Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable HDPE by gas injectionInformation provided .. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Westlake EMAC® Plus SP1330 22% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1330 is a 22% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1330 is.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formula.. |
|||
Density | 0.948 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |