Material Notes:
Westlake EMAC® Plus SP1330 is a 22% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1330 is compatible with and provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance. The higher melting point of this EMAC®Plus grade offers EMA performance with improved heat resistance.Applications: films, disposable gloves, and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Methyl Acrylate Content 22 %
22 %
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 37
37
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 865 %
865 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
by DSC; ASTM D3418
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Blown Film
Extrusion
Film
Region US & Canada