Material Notes:
Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes Applications: Hot Melt AdhesivesWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ExxonMobil method
Vinyl Acetate Content 28 %
28 %
ExxonMobil method
Melt Flow 400 g/10 min
400 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Molded Properties; ASTM D2240
Tensile Strength at Break 2.48 MPa
360 psi
(20 in/min), Molded Properties; ASTM D638
Elongation at Break 570 %
570 %
(20 in/min), Molded Properties; ASTM D638
Tensile Modulus 0.0117 GPa
1.70 ksi
(0.2 in/min), Molded Properties; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 156 °C
<= 313 °F
Peak Melting Point; ExxonMobil method