Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.944 g/cc | 0.0341 lb/in³ | Compression Molded; ASTM D792 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. I.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Density | 0.944 - 0.950 g/cc | 0.0341 - 0.0343 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HD 7555 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene EX1 (HF 7740F2) is high density polyethylene with Butene-1 as co monomer. It is a medium molecular mass with a narrow molar mass distribution.Application: stretched film tape used in manufacture o.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 (Natural) |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Density | 0.944 - 0.948 g/cc | 0.0341 - 0.0342 lb/in³ | DIN 53479 |
Iran Petrochemical (PCC) Arak BL2 HDPE Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2590 is a high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization is optimized .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Natural; ASTM D1505 |
Formosa Plastics Formolene® HP4401 Pipe HDPE High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requiremen.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | masterbatch; ASTM D-1505 |
Chevron Phillips Marlex® M368 Polyethylene; Masterbatch This black masterbatch with its medium density polyethylene (MDPE) carrier resin has been formulated for pipe applications that require: Good long-term hoop strengthExtended outdoor lifeClean N550 .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | natural resin; ASTM D792 |
Dow DGDB-2480 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM-D792 |
Braskem GM7746C HDPE Blow Molding Polyethylene GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM-D792 |
Braskem GM7746CA HDPE Blow Molding Polyethylene GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Natural; ASTM D1505 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2591 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, offering excellent processability for peroxide crosslinking. It is a special polymer, stabilized .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Density; ASTM D1505 |
Chevron Phillips Marlex® M362 LLDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strengthExtended outdoor lifeClean N550 carbon blackApplications: PipesNot recommended for contact with food productsInformation provided by Chevron Phillips. |