Material Notes:
K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; some physical properties may be specific to the carbon black filled resin.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
Condition C; ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 22.8 MPa
3310 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 0.793 GPa
115 ksi
2% Secant-Method 1; ASTM D790
Izod Impact, Notched 5.30 J/cm
9.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Descriptive Properties Value Comments
Process Pipe Extrusion
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved