Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.910 g/cc | 0.0329 lb/in³ | |
Plastcom SLOVALEN PQ 83 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Hyosung Topilene HJ700 PP HJ700 High Isostatic PP HomopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceInformation provided by Hyosung Corporation |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | 9700B |
Lord Adhesives Aeroglaze® 9743 Epoxy Primer/Tie-Coat Aeroglaze® 9743 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9743 primer/tie-coat can be applied to scuff-sanded urethane top coats a.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | 9700B |
Lord Adhesives Aeroglaze® 9744 Epoxy Primer/Tie-Coat Aeroglaze® 9744 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9744 primer/tie-coat is applied to scuff-sanded urethane top coats and e.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Mitsui ADMER® NF488A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 5703 BLK The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505-98 |
Ipiranga Petrochem LTH 0212 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Microstructure: cis: 96trans: 2vinyl: 2Information provided by UBE. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products. Stabilizer Type: Non-stainingMicrostructure: cis: 98trans: 1vinyl: 1Information provided by UBE. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
UBE UBEPOL VCR303 Synthetic Rubber (Raw Polymer) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Borealis HJ325MO Polypropylene HJ325MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. is designed fo.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Borealis WG320C Polypropylene WG320C is a polypropylene for extrusion coating. Applications: microwave oven applications, pinholes free coating, extrusion coating of high volume production of boards and papers, coating of texti.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Domo 1101S Polypropylene Homopolymer Information provided by Domo. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Domo 1102J Polypropylene Homopolymer Information provided by Domo. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Domo 1102M Polypropylene Homopolymer Information provided by Domo. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Domo 2600PC Polypropylene Copolymer Information provided by Domo. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
Dow AFFINITY™ PL 1845 Polyolefin Plastomer Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Density | 0.910 g/cc @Temperature 15.6 °C |
0.0329 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 636 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Density | 0.910 g/cc @Temperature 15.6 °C |
0.0329 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 600 W Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Density | 0.910 g/cc @Temperature 23.0 °C |
0.0329 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1102 H Polypropylene Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.910 - 0.942 g/cc | 0.0329 - 0.0340 lb/in³ | Average value: 0.921 g/cc Grade Count:84 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1125 N Polypropylene Cast film with medium slip.Data was collected by ISO methods and provided by BASF. |