| Category | Polymer , Film , Thermoplastic , Elastomer, TPE |
| Manufacturer | Dow Chemical |
| Trade Name | AFFINITY™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow AFFINITY™ PL 1845 Polyolefin Plastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.910 g/cc | 0.0329 lb/in³ | |
| Thickness | 25.0 microns | 0.984 mil | |
| Melt Flow | 3.5 g/10 min @Load 2.16 kg |
3.5 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Elongation at Break, MD | 527 % | 527 % | |
| Film Elongation at Break, TD | 664 % | 664 % | |
| Elmendorf Tear Strength MD | 178 g | 178 g | |
| Elmendorf Tear Strength TD | 362 g | 362 g | |
| Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | |
| Elmendorf Tear Strength, TD | 14.5 g/micron | 368 g/mil | |
| Dart Drop | 18.8 g/micron | 478 g/mil | |
| Film Tensile Strength at Break, MD | 45.4 MPa | 6580 psi | |
| Film Tensile Strength at Break, TD | 33.4 MPa | 4840 psi |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 0.70 % | 0.70 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 99.0 °C | 210 °F | Seal initiation temperature |
| 274 °C | 525 °F | Film extrusion temperature |