Dow Engage® 8445 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Dow Chemical
Trade Name Engage®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Engage® 8445 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other polyolefins, allowing for efficient blending and coextrusion. Engage® 8445 provides excellent flow properties and is efficiently cross-linked by peroxide, silane, or irradiation. When cross-linked, it gives exceptional heat aging, compression set, and weather resistance properties. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Index of Compound 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Hardness, Shore D 41
41
ASTM D2240
Tensile Strength, Ultimate 21.0 MPa
3050 psi
508 mm/min; ASTM D638
Tensile Strength, Yield 8.30 MPa
1200 psi
508 mm/min; ASTM D638
Elongation at Break 800 %
800 %
508 mm/min; ASTM D638
2% Secant Modulus 0.1101 GPa
15.97 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 103 °C
217 °F
DSC, 10°C/min; DuPont Test
Vicat Softening Point 93.0 °C
199 °F
ASTM D1525
Descriptive Properties Value Comments
Comonomer Content 16 wt%
Dow Method (<sup>13</sup>C NMR/FTIR)