Material Notes:
Neoplast 173 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D 2240
77

@Treatment Temp. 150 °C,
Time 605000 sec
77

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 6.37 MPa
925 psi
500 mm/min; ASTM D 412
7.06 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
1020 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 200 %
200 %
500 mm/min; ASTM D 412
176 %

@Treatment Temp. 150 °C,
Time 605000 sec
176 %

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00539 GPa
0.782 ksi
500 mm/min; ASTM D 412
Tear Strength 27.5 kN/m
157 pli
500 mm/min; ASTM D 624
Compression Set 40 %

@Temperature 70.0 °C,
Time 79200 sec
40 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; SAE J 2236
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D 746