Zotefoams Evazote® VA65 Ethylene Vinyl Acetate Copolymer Foam

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Zotefoams
Trade Name Evazote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams Evazote® VA65 Ethylene Vinyl Acetate Copolymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Compliant with EC food contact and US FDA regulations.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0650 g/cc
0.00235 lb/in³
Nominal skin/skin; BS ISO 7214 1998
0.0570 - 0.0740 g/cc
0.00206 - 0.00267 lb/in³
sheet density
Cell Length 0.670 mm
0.0264 in
Typical Diameter
0.500 - 0.900 mm
0.0197 - 0.0354 in
Mechanical Properties Metric English Comments
Hardness, Shore OO 60
60
10 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.825 MPa
120 psi
ISO 7214 1998
Elongation at Break 185 %
185 %
Compressive Yield Strength 0.0680 MPa

@Strain 10.0 %
9.86 psi

@Strain 10.0 %
BS ISO 7214 1998
0.0890 MPa

@Strain 25.0 %
12.9 psi

@Strain 25.0 %
BS ISO 7214 1998
0.123 MPa

@Strain 40.0 %
17.8 psi

@Strain 40.0 %
BS ISO 7214 1998
0.162 MPa

@Strain 50.0 %
23.5 psi

@Strain 50.0 %
BS ISO 7214 1998
Tear Strength 1.59 kN/m
9.07 pli
BS EN ISO 8067 1995
Compression Set 2.0 %

@Time 79200 sec,
Strain 25.0 %
2.0 %

@Time 22.0 hour,
Strain 25.0 %
24 hr recovery; BS ISO 7214 1998
5.5 %

@Time 79200 sec,
Strain 25.0 %
5.5 %

@Time 22.0 hour,
Strain 25.0 %
0.5 hr recovery; BS ISO 7214 1998
6.0 %

@Time 79200 sec,
Strain 50.0 %
6.0 %

@Time 22.0 hour,
Strain 50.0 %
24 hr recovery; BS ISO 7214 1998
15 %

@Time 79200 sec,
Strain 50.0 %
15 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; BS ISO 7214 1998
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Flammability Test 0.80

@Thickness 13.0 mm
0.80

@Thickness 0.512 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
1.0

@Thickness 5.00 mm
1.0

@Thickness 0.197 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
Descriptive Properties Value Comments
Flammability Automotive: FMVSS.302 burn rate
Pass: 3mm and thicker