Material Notes:
General-purpose, intermediate viscosity nitrile rubber for industrial and automotive hose and seals, printing rolls and applications requiring easy processing.General purpose, intermediate-viscosity nitrile rubber for industrial and automotive hose and seals, printing rolls, and applications requiring easy processing.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Mooney Viscosity 42 - 52

@Temperature 100 °C
42 - 52

@Temperature 212 °F
(1+4)
Ash <= 0.75 %
<= 0.75 %
T-4210
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 29-31
Heat Loss (%) Max 0.5
Hot/Cold C