Zeon Chemicals Hydrin® C2000 Polyepichlorohydrin Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Hydrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Hydrin® C2000 Polyepichlorohydrin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrin C2000 is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Fuel pump diaphragms, hose, coated fabrics and vibration mounts. Can also impart antistatic properties to plastics.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Mooney Viscosity 90 - 102

@Temperature 100 °C
90 - 102

@Temperature 212 °F
(1+4)
Ash <= 1.0 %
<= 1.0 %
Zeon Test #1358
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Component Elements Properties Metric English Comments
Chlorine, Cl 24.5 - 26.5 %
24.5 - 26.5 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361