Polymer Property : Glass Transition Temp, Tg = -41.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Zeon Chemicals Hydrin® C2000 Polyepichlorohydrin Elastomer
Hydrin C2000 is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000 typically exhibit good heat resistance, excellent ozone resistanc..
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Zeon Chemicals Hydrin® C2000L Polyepichlorohydrin Elastomer
Hydrin C2000L is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000L typically exhibit good heat resistance, excellent ozone resista..
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Zeon Chemicals Hydrin® C2000LL Polyepichlorohydrin Elastomer
Hydrin C2000LL is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000LL typically exhibit good heat resistance, excellent ozone resis..
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Zeon Chemicals Hydrin® C2000XL Polyepichlorohydrin Elastomer
Hydrin C2000XL is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000XL typically exhibit good heat resistance, excellent ozone resis..
Glass Transition Temp, Tg -41.0 °C
-41.8 °F
Zeon Chemicals Hydrin® T3105 Polyepichlorohydrin Elastomer
Hydrin T3105 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil fuel and solvent resistance. Compounds using Hydrin T3105 typically exhibit excellent low and high tem..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..