Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Pomalux® Acetal Copolymer, Compression Molded

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Westlake Plastics
Trade Name Pomalux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Pomalux® Acetal Copolymer, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compression molded Pomalux is a high performance acetal copolymer with excellent mechanical, electrical, and wear properties. Pomalux has excellent dimensional stability even with complex geometries. As a bearing surface, it works well in dry and wet applications. Pomalux is FDA compliant. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D7852
Tensile Modulus 2.62 GPa
380 ksi
ASTM D638
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.52 mm
HB

@Thickness 0.0600 in
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
ASTM D150