Material Notes:
WESTLAKE HIFOR Xtreme SC74859 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and high processing aid.Application/UsesFresh produce packagingFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.60 g/10 min
0.60 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 750 %
750 %
ASTM D882
Film Elongation at Break, TD 1150 %
1150 %
ASTM D882
Dart Drop 5.91 g/micron
150 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Film Tensile Strength at Break, TD 43.4 MPa
6300 psi
ASTM D882
1% Secant Modulus, MD 248 MPa
36000 psi
ASTM D882
1% Secant Modulus, TD 317 MPa
46000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 17 %
17 %
ASTM D1003
Gloss 55 %
55 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 204 - 216 °C
400 - 420 °F
Blow-up Ratio (BUR) 2.4
2.4
Descriptive Properties Value Comments
Process Blown Film
Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: