Material Notes:
WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Application/UsesMilk CartonsLiquid ContainersMultiwall bag stockFrozen food containersFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 5.7 g/10 min
5.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Tensile Modulus 0.165 GPa
24.0 ksi
ASTM D1709
Processing Properties Metric English Comments
Melt Temperature 302 - 329 °C
575 - 625 °F
Descriptive Properties Value Comments
Process Coating