Universal Wire Works A Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works A Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy A is used for arc welding various dissimilar combinations of austenitic and ferritic steels and high nickel alloys. For example, when welding Inconel and Incoloy type alloys to carbon steel, stainless steel, Nickel 200, Monel type alloys, and nickel alloys, it is the product of choice. Alloy A is used to weld Monel type alloys, Nickel 200, and carbon steel to stainless steels. Alloy A is recommended for welding Incoloy type alloy 800 and 9% nickel steel to themselves. Electrode sizes 3/32 and 3/16 diameter can be used in all positions, while the larger 5/32 and 3/16 diameter are normally used in the flat or horizontal positions. POWER SUPPLY DCRP.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 13 - 17 %
13 - 17 %
Cobalt, Co <= 0.12 %
<= 0.12 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 12 %
<= 12 %
Manganese, Mn 1.0 - 3.5 %
1.0 - 3.5 %
Nickel, Ni >= 62 %
>= 62 %
Niobium, Nb (Columbium, Cb) 1.0 - 2.5 %
1.0 - 2.5 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.020 %
<= 0.020 %
Tantalum, Ta <= 0.30 %
<= 0.30 %
Titanium, Ti <= 1.0 %
<= 1.0 %