Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UPIMOL® SA201 Heat-Resistant Polyimide Shape

Category Polymer , Thermoset , Polyimide, TS
Manufacturer UBE
Trade Name UPIMOL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UPIMOL® SA201 Heat-Resistant Polyimide Shape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UPIMOL SA201 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL SA201 can save costs, and suit various applications.Applications: Semiconductor production equipment partsLCD panel production equipment partsVacuum equipment partsPrecisely processed partsHeat and chemical resistant gaskets and sealing materialsFeatures: Super high heat resistance (Heat distortion temperature: 486°C)Suitable for high vacuum conditionGood processabilityVery low impuritiesInformation provided by UBE.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.34 g/cc
1.32 - 1.34 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ASTM D785
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 4.4 %
4.4 %
ASTM D638
Flexural Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 25.0 - 450 °C
27.8 µin/in-°F

@Temperature 77.0 - 842 °F
ASTM E233
Maximum Service Temperature, Air 486 °C
907 °F
Heat Distortion Temp, Load Unknown; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 7.10e+15 ohm-cm
7.10e+15 ohm-cm
ASTM D257
Surface Resistance 1.60e+15 ohm
1.60e+15 ohm
ASTM D257
Dielectric Constant 3.51

@Frequency 1e+6 Hz
3.51

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.7 kV/mm

@Temperature 25.0 °C
323 kV/in

@Temperature 77.0 °F
Breakdown Voltage; ASTM D149
Dissipation Factor 0.0031

@Frequency 1e+6 Hz
0.0031

@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Vacuum Degassing 3.3 x 10-6Torr x l/sec x cm2
TDS Analysis at 300°C
4.5 x 10-6Torr x l/sec x cm2
TDS Analysis at 200°C