Material Notes:
TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resistance, while maintaining excellent antistatic properties and good processability.Total Polypropylene 4524WZ has been developed specifically for the injection molding of baskets, pails, toys and any articles requiring extra toughness.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm

@Temperature -20.0 °C
1.31 ft-lb/in

@Temperature -4.00 °F
ASTM D256
1.88 J/cm

@Temperature 23.0 °C
3.52 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Pressure unspecified; ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525