Physical Properties Metric English Comments
Specific Gravity 0.971 g/cc
0.971 g/cc
Viscosity 12 cP

@Temperature 100 °C
12 cP

@Temperature 212 °F
132 cP

@Temperature 40.0 °C
132 cP

@Temperature 104 °F
Viscosity Measurement 83.0
83.0
Viscosity Index
Thermal Properties Metric English Comments
Pour Point -35.0 °C
-31.0 °F
Flash Point 282 °C
540 °F
Chemical Properties Metric English Comments
Acid Value <= 0.10
<= 0.10
mg KOH/g
Descriptive Properties Value Comments
Appearance Clear
Color 100
Pt/Co Scale
Ester Content (%), min 99
Moisture (ppm), max 500