Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.971 - 0.981 g/cc @Temperature 25.0 °C |
0.971 - 0.981 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ TINTM-E Triisononyl Trimellitate Branched C9 trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Specific Gravity | 0.971 g/cc | 0.971 g/cc | |
Northstar Polymers YPX-164 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 0.971 g/cc | 0.971 g/cc | |
Teknor Apex TruVis Esters™ TIDTM Tri-Isodecyl Trimellitate |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning Q7-9120 Silicone Fluid, 350 CST Polydimethylsiloxane fluid, excipient for pharmaceutical and cosmetic applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 30,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 30,000CS. 100% active, 30,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 500CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 500CS. 100% active, 500 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning 200® 1000 CST FLUID 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 1000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 1,000CS. 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.971 g/cc @Temperature 25.0 °C |
0.971 g/cc @Temperature 77.0 °F |
|
Dow Corning 360 Medical Fluid, 350 CST. Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning |