Teknor Apex Synres® PP 70 MH13 MB Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Teknor Apex Company
Trade Name Synres®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Synres® PP 70 MH13 MB Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: The Specialty Compounding Division offer a proprietary line of flame retardant polyolefins. Typical applications include building products, electrical/electronic and many other consumer and industrial applications. These compounds can be tailored to specific needs and are available pre-colored or natural. Product Description: 70% Magnesium Hydroxide Masterbatch Features: Flame Retardant Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Melt Flow 4.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
10 seconds; ASTM D2240
Flexural Modulus 4.07 GPa
590 ksi
ASTM D790
Izod Impact, Notched 0.107 J/cm
0.200 ft-lb/in
ASTM D256