Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: General Purpose; OpaqueInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 3.00 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.00 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM D2240
Tensile Strength at Break 4.14 MPa
600 psi
ASTM D412
Tensile Strength, Yield 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412