Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 4.14 MPa | >= 600 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | Oven cured 4 hours at 480°F |
Malvern Minerals Sliastic 740 with 33% Novacite® L-207A Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 4.14 MPa @Time 7200 sec |
600 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7345-9000 TPE Product Description: StarFlex P 7345-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP 1870 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP-2111 L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP-2290 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer Notes: General Purpose; OpaqueInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | 20 in/min; ASTM D412 |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1366A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1366C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Monprene® MP-2850A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D412 |
Teknor Apex Telcar® TL-1081A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | 20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | Die A; ASTM D412 |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | Die A; ASTM D412 |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | Die A; ASTM D412 |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | Die A; ASTM D412 |
3M Bumpon™ SJ6232 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Tensile Strength at Break | 4.14 MPa | 600 psi | ASTM D882 |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Tensile Strength at Break | >= 4.14 MPa | >= 600 psi | Gasoline Resistance |
3M TMW Tubing 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th.. |