Teknor Apex APEX® 1700-60 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 1700-60 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Method-Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746