Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.FormulationMillathane 97 100.0Stearic Acid0.3Wacker HDK N20 (fumed silica)20.0Luperox 2310.4SR-231 (DEGDMA)3.0Irganox 10100.2All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Yield 22.6 MPa
3280 psi
Elongation at Yield 555 %
555 %
100% Modulus 0.00159 GPa
0.230 ksi
200% Modulus 0.00221 GPa
0.320 ksi
300% Modulus 0.00338 GPa
0.490 ksi
Tear Strength 30.4 kN/m
173 pli
Die C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 8.00 min

@Temperature 149 °C
0.133 hour

@Temperature 300 °F
Users viewing this material also viewed the following: