TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5SR-2977.5Hi-Sil 23325.0AC Poly 617A2.0Di-Cup 40C3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 23.04 MPa
3341 psi
Elongation at Yield 296 %
296 %
100% Modulus 0.00556 GPa
0.807 ksi
200% Modulus 0.01209 GPa
1.754 ksi
Tear Strength 35.4 kN/m
202 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 160 °C
0.250 hour

@Temperature 320 °F
Users viewing this material also viewed the following: