Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 35.4 kN/m | 202 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 35.3 kN/m | 202 pli | |
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/40 Polyurethane Casting Elastomer Compound of CPU-69-A/B with a mixing ratio of 100/40.Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components. |
|||
Tear Strength | 35.4 kN/m | 202 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 35.4 kN/m | 202 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 35.4 kN/m | 202 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 35.4 kN/m | 202 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 35.4 kN/m | 202 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |