TIMCAL TIMREX® T15 Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® T15 Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.100 g/cc
0.00361 lb/in³
Scott
Particle Size 17.7 µm
17.7 µm
d90, Typical
15.5 - 20.5 µm
15.5 - 20.5 µm
d90, Guaranteed
Specific Surface Area 13 m²/g
13 m²/g
BET
Ash 0.080 %
0.080 %
Typical
<= 0.10 %
<= 0.10 %
Guaranteed
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Typical
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Aspect Fine black powder
Crystallinity, Lc, nm 90
Crystallite Height, nm minimum 80
Interlayer Distance, nm .3354-.3360