Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 15.5 - 20.5 µm | 15.5 - 20.5 µm | d90, Guaranteed |
TIMCAL TIMREX® T15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 15.5 - 20 µm | 15.5 - 20 µm | d90, Guaranteed |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |