Material Notes:
Blend fatty acid derived and functional inorganic materials.Applications: STRUKTOL® VCS-526A is recommended for us with recycled rigid PVC where additional stabilization and lubrication is needed to reduce yellowing, burning and sticking in extrusion, injection molding and calendering. It is especially useful in allowing higher loadings of PVC regrind (post industrial or post consumer) in virgin formulations. It also allows for longer production runs between shutdowns due to degradation.Information provided by Struktol
Physical Properties Metric English Comments
Specific Gravity 1.113 g/cc
1.113 g/cc
Additive Loading 0.50 - 2.0 %
0.50 - 2.0 %
Ash 29 - 35 %
29 - 35 %
Thermal Properties Metric English Comments
Dropping Point 142 - 147 °C
288 - 297 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance White to pale yellow pellets