Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.113 g/cc | 1.113 g/cc | |
Struktol VCS 526A Co-Stabilizing Processing Additive Blend fatty acid derived and functional inorganic materials.Applications: STRUKTOL® VCS-526A is recommended for us with recycled rigid PVC where additional stabilization and lubrication is needed.. |