Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Struktol TR 141 Slip Agent, Lubricant, Mold Release Agent

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TR 141 Slip Agent, Lubricant, Mold Release Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A saturated primary amide with no double bond.STRUKTOL® TR 141 stearamide is a saturated primary amide with no double bond. It blooms in an invisible monolayer for surface appearance and mold release. It can also be used for viscosity reduction. STRUKTOL® TR 141 is relatively insoluble in water and has limited solubility in alcohol, ketones and aromatic solvents. STRUKTOL® TR 141 will not interfere with peroxide cure systems in cross-linked polymer systems.FDA Status: 175.105; 177.1210; 178.3910; 179.45; 181.28
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Additive Loading 0.50 - 1.0 %
0.50 - 1.0 %
For plastics (1-3 phr in elastomers)
Thermal Properties Metric English Comments
Melting Point 98.0 - 104 °C
208 - 219 °F
Optical Properties Metric English Comments
Gardner Color Number 5.0
5.0
Chemical Properties Metric English Comments
Acid Value <= 9.0
<= 9.0
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Cream colored beads or pellets.