Spartech SP-2050 Glossy HIPS Polystyrene Sheet

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SP-2050 Glossy HIPS Polystyrene Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polystyrene SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell L 55
55
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Falling Dart Impact 9.04 J
6.67 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523