Polymer Property : Flexural Yield Strength = 48.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 48.3 - 2000 MPa
7000 - 290000 psi
Average value: 300 MPa Grade Count:182
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Flexural Yield Strength 48.3 - 280 MPa
7000 - 40600 psi
Average value: 124 MPa Grade Count:49
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Flexural Yield Strength 48.3 - 110 MPa
7000 - 16000 psi
Average value: 84.8 MPa Grade Count:6
Overview of materials for Polyphenylene Ether, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values..
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet
Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Spartech Royalite R20 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Flexural Yield Strength 48.3 MPa
7010 psi
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet
Data provided by the manufacturer.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Spartech Royalstatâ„¢ R632 ABS/PVC Static Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Spartech SP-2010 HIPS Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Spartech SP-2050 Glossy HIPS Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Techmer ES Luriblend® TPX-HDPE-99018
Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc.
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Westlake Plastics Clariflex® TFE/VF2/HFP
Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance..
Flexural Yield Strength 48.3 MPa
7010 psi
ASTM D790
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Yield Strength 48.3 MPa
7010 psi
ASTM D790
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Yield Strength 48.3 MPa
7010 psi
ASTM D790
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 48.3 MPa
7010 psi
ASTM D790
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Yield Strength 48.3 - 80.0 MPa
7000 - 11600 psi
Average value: 65.6 MPa Grade Count:7
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Flexural Yield Strength 48.3 MPa
7010 psi
ASTM D790
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 48.3 - 124 MPa
7000 - 18000 psi
Average value: 94.3 MPa Grade Count:131
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..