Solvay Specialty Polymers Polymist® XPP 552 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® XPP 552 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® XPP 552 is a white PTFE micronized powder composed of discrete particles. Designed for use in critical engineering and high end performance Coatings and Inks, Polymist® XPP 552 will improve non-stick properties, mar and abrasion resistance as well as slip and rub resistance.Uses: AdditiveAdditional Properties: Average Particle Size - Internal Method 3.3 µm; Average Particle Size - Internal Method 8.0 µm; Bulk Density - ASTM D4895 > 325 g/l; Grind in Oil - NPIRI 1.50; Melt Temperature - ASTM D3418 320 to 330 °C; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder