Solvay Specialty Polymers Hyflon® MFA® XPH 5510_1N Perfluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer , TFE/Perfluoromethylvinylether Copolymer (MFA)
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon® MFA®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® MFA® XPH 5510_1N Perfluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hyflon® XPH 5510_1N is a white aqueous MFA dispersion. Hyflon® XPH 5510_1N exhibits excellent wetting properties and high shear stability. Hyflon® XPH 5510_1N has very good film forming behavior and is especially suited for top-coat passes to produce final items with superior gloss. Due to its features, XPH 5510_1N can of course also find use in formulations for coating applications.Features: High Gloss; Rapid WettingUses: Coating Applications; Impregnation ApplicationsAdditional Properties: Average Particle Size - Internal Method 0.18 µm; Brookfield Viscosity - ASTM D2196 (20°C): 20 mPa·s; MFA Content - ASTM D4441 55.0 wt%; Non Ionic Surfactant - ASTM D4441 3.5 wt%; pH - ASTM D4441 > 9.0Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D1505
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
DSC
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color White
Form Liquid