Solvay Specialty Polymers Diofan® A 297 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 297 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Diofan® A 297 is a latex with high surface tension for high speed processing, in particular designed for coating on plastic films, but also suitable to be applied on other substrates.Features: Moisture Barrier; Oxygen BarrierUses: Barrier Coatings; Coating ApplicationsAdditional Properties: Density - 1.650 g/cm³; Density - 1.330 g/cm³; Emulsion Type - Anionic; Filmability - 8 to 14 °C; Heat Seal Maximum Resistance - 2.5 N/cm; Heat Seal Threshold - 111 °C; Oxygen Transmission Rate - ASTM D3985 40 cm³/m²/bar/24 hr; pH - 1.5; Shelf Life - (23°C): 10 month; Solids Content - 60 %; Surface Tension - 54 mN/mInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 14.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
0.902 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.30
0.30
vs. Itself; ASTM D1894
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid